Oil Change - What to Look For

A Ducati engine has a filter to remove microscopic and larger particles from the circulating oil, a magnet on the oil drain plub to remove any particles of magnetic material such as iron and steel, and has a removable mesh screen to capture larger non-magnetic metals such as aluminum and chromium as well as other non-metals such as gasket material. Each time you change your oil you should check your engine’s heath by examining them for any unusual amounts of material. This is probably the best reason to change your own oil.

If you've ever seen metal being machined, you'll know that metal chips and machining oil gets everywhere. The finished part is always then sent to a cleaning operation where most of the chips are flushed out of all the tiny crevices. But there's ALWAYS some particles left in complex shapes with internal oil and water passages such as an engine casing. That's why you have both a oil screen for big particles and an oil filter for small ones.

So, seeing a larger number of particles on your drain magnet and oil screen should be expected for the first few oil changes, and then seen to decrease over time unless there’s a problem. Here’s a way to diagnose problems.

Drain Plug Magnet



It’s common to see fingernail-clipping size magnetic particles from normal transmission gear wear. Anythine larger should be a concern. Fuzz-like smaller particles on the plug are from normal wear of scores of moving parts, so they should be expected.

Oil Screen

Since it’s normal to see aluminum particles from machining operations show up initially on the screen filter, it’s important to know about common problems with Ducati engines that also result in particles on the oil screen.


Paul Yoshimune photo


70cuda Photo

The first problem is that the oil galley plug on pre-2001 model year engines were made of aluminum and would unscrew causing a catastrophic loss of oil pressure that results in big-end bearing failure.

When the plug backs out, it backs into the outer race of the left side crankshaft bearing. The race, being much harder than the aluminum, basically machines down the plug a little at a time until the sliver of the plug drops into the crankcase of the motor and the oil pressure light comes on. At that point, the oil pressure is used to pump the oil through the crankshaft and no oil gets to the rod bearings, crank bearings, or upper end of the motor - because those places all require oil under pressure.

In 2001 steel plugs were introduced that solved this problem but if you have an earlier bike you need to watch for an unusual amount of aluminum particles on the screen. If you spot it in time, you can split the engine case and replace the plug before there is any subsequent damage. It takes awhile for the plug to machine itself off and back-out completely.

To confirm the problem you need to remove the vertical cylinder, pull up on the connecting rod, and look to the left of the rod. If there's a dull silver part of the crankshaft touching the outer race of the crankshaft bearing, you got the problem. The plug should be flush or slightly inset.

The second problem is the design problem with the chrome plating flaking-off the cam-contacting surface of the rocker arms. The best way to know if you have rocker problems is to pull the cams and look, but your dealer won't do this unless you authorize an additional labor charge. Chrome particles on the filter screen will give you a good reason to spend the money to have them do this.

Chrome and aluminum are non-magnetic so they don’t attach themselves to the magnet on the drain plug. So how do you tell if you have chrome or aluminum particles on your filter screen? Here’s a simple test.

The Test

Draw a small amount of battery acid and put the particles in it. Battery acid is dilute sulfuric acid, so when you add chromium to it you’ll get a release of hydrogen bubbles and the chromium will turn the darker violet color of chromium sulfate. Aluminum doesn’t react this way.

For you chemistry majors:

2Cr + 3H2SO4 > Cr2 [SO4]3 + 3H2



[Edited on 7-22-2005 by Shazaam!]

Last edited by Shazaam! : 08-Feb-2009 at 01:46.
Quote+Reply
  #2  
Old 21-Jul-2005, 20:58
Dibble
 
Posts: n/a
you bored ???

superbly informative though.

cheers
Quote+Reply
  #3  
Old 21-Jul-2005, 21:06
phil_h's Avatar
phil_h phil_h is offline
Registered Forum User
Ducati Meccanica
 
Posts: 2,527
Join Date: Sep 2004
Mood: 900,900,851,750,750,750, 600,600,450,350,350,250
Good description - what happens to the oil when you drop it into the acid though ?
Doesnt that also produce some gunk that can hide what you're looking for ?
Quote+Reply
  #4  
Old 22-Jul-2005, 12:36
Derek's Avatar
Derek Derek is offline
Registered Forum User
GTL
Bikes: ST4s ABS
 
Posts: 480
Join Date: Aug 2003
Quote:
Originally posted by Shazaam!
non-magnetic metals such as aluminum and chromium
Chromium is in fact magnetic. The five magnetic elements are manganese, nickel, chromium, iron and cobalt.
Quote+Reply
  #5  
Old 22-Jul-2005, 16:43
Shazaam!'s Avatar
DSC Member Shazaam! Shazaam! is offline
DSC Club Member
Big Twin
 
Posts: 1,167
Join Date: Nov 2001
Correct me if I'm wrong but it is my understanding here are only three elemental ferromagnetic substances; iron, nickel, and cobalt. The element chromium is not ferromagnetic, but becomes more ferromagnetic than iron oxide as Chromium(IV) oxide (CrO2), which is commonly used in recording tape. Manganese becomes ferromagnetic (only) after special treatment. However, combined with aluminum and antimony, especially in the presence of copper, it forms highly ferromagnetic alloys.
Quote+Reply
  #6  
Old 22-Jul-2005, 17:40
Derek's Avatar
Derek Derek is offline
Registered Forum User
GTL
Bikes: ST4s ABS
 
Posts: 480
Join Date: Aug 2003
I thought I had you there

Actually Chromium and Manganese are weak ferromagnetics. See http://www.iop.org/EJ/abstract/0959-5309/48/5/311
As you say the magnetic susceptibility of Chromium is greatly increased by the addition of impurities.
Quote+Reply
  #7  
Old 22-Jul-2005, 18:29
stephen hall's Avatar
stephen hall stephen hall is offline
Registered Forum User
Mille
 
Posts: 210
Join Date: Nov 2003
someone gis a shake

Quote+Reply
  #8  
Old 22-Jul-2005, 19:19
Davieravie's Avatar
Davieravie Davieravie is offline
Registered Forum User
500SD
 
Posts: 799
Join Date: Jul 2005
Mood: Warmed up and ready to go
Nice bedtime reading this.
Quote+Reply
  #9  
Old 23-Jul-2005, 17:29
philthy's Avatar
philthy philthy is offline
Registered Forum User
Big Twin
 
Posts: 1,028
Join Date: Jun 2005
Mood: Can't make me mind up
Mine's an 89 model and I'm frightened to ride the bl***y thing now
in case it blows up!
Quote+Reply
  #10  
Old 24-Jul-2005, 00:08
phil_h's Avatar
phil_h phil_h is offline
Registered Forum User
Ducati Meccanica
 
Posts: 2,527
Join Date: Sep 2004
Mood: 900,900,851,750,750,750, 600,600,450,350,350,250
Quote:
The first problem is that the oil galley plug on pre-2001 model year engines were made of aluminum and would unscrew causing a catastrophic loss of oil pressure that results in big-end bearing failure.

Thats quite an open ended quote isnt it.
That crank design started life in the pantah engines ... and must be in the f1, 906, 907, 851, 888.
Why have we never heard of the problem ?
Was it used _starting_ from a particular year too ?
Quote+Reply
Reply
  
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes
Postbit Selector
Switch to Vertical postbit Use Vertical Postbit

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Recent Posts - Contact Us - DSC Home - Archive - Top
Powered by vBulletin 3.5.4 - Copyright © 2000 - 2024, Jelsoft Enterprises Ltd. - © Ducati Sporting Club UK - All times are GMT +1. The time now is 14:47.